Statistical analysis of yield strength spectrum from nanoindentation for identification of constituent phases in steel
Auteur(s): |
Thai-Hoan Pham
Ngoc-Vinh Nguyen |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | IOP Conference Series: Materials Science and Engineering, juillet 2020, v. 869 |
Conférence: | XXIII International Scientific Conference on Advance in Civil Engineering: "CONSTRUCTION - THE FORMATION OF LIVING ENVIRONMENT" (FORM-2020) 23-26 September 2020, Hanoi, Vietnam |
Page(s): | 052038 |
DOI: | 10.1088/1757-899X/869/5/052038 |