Alkali-activated materials were prepared from pond ash from the Darkhan city (Mongolia) thermal power station. This ash contains about 60 wt % X-ray amorphous material in addition to quartz, mullite, hematite and magnesioferrite, and presents significant storage problems since it is accumulating in large amounts and is a hazardous waste, containing 90–100 ppm of the heavy metals As, Pb and Cr, and about 800 ppm Sr. Alkali-activated materials synthesized from the as-received pond ash achieved compressive strengths of only 3.25 MPa. Reduction of the particle size by mechanical milling for up to 30 min progressively increases the compressive strength of the resulting alkali-activated geopolymer up to 15.4 MPa. Leaching tests indicate that the combination of milling and alkali treatment does not cause the release of the hazardous heavy metals from the product, making it suitable for construction applications.

Structurae ne peut pas vous offrir cette publication en texte intégral pour l'instant. Le texte intégral est accessible chez l'éditeur. DOI: 10.3989/mc.2017.07716.
  • Informations
    sur cette fiche
  • Reference-ID
    10516970
  • Publié(e) le:
    10.12.2020
  • Modifié(e) le:
    19.02.2021
 
Structurae coopère avec
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine