A novel method for steel bar all-stage pitting corrosion monitoring using the feature-level fusion of ultrasonic direct waves and coda waves
Auteur(s): |
Xiangtao Sun
(Department of Disaster Mitigation for Structures, Tongji University, Shanghai 200092, China)
Minghui Zhang (Department of Disaster Mitigation for Structures, Tongji University, Shanghai 200092, China) Weihang Gao (Department of Disaster Mitigation for Structures, Tongji University, Shanghai 200092, China) Chuanrui Guo (College of Civil and Transportation Engineering, Institute of Urban Smart Transportation & Safety Maintenance, Shenzhen University, Shenzhen 518060, China) Qingzhao Kong |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Structural Health Monitoring, novembre 2019, n. 1, v. 22 |
Page(s): | 147592172210944 |