Abstrait:

In this paper the impact of carbonate-containing and sulfate components, zeolite, polypropylene fibers on the properties of modified binding composition and non-autoclaved aerated concrete based on them is investigated. The aerated concrete based on the modified binding composition containing a supplementary cementitious material, that of carbonate-containing salt waste, reinforced with polypropylene fibers is characterized by the compressive strength of 2.7 MPa with the density of 650 kg/m³. The thickness of partitions between pores is 0.16 – 0.21 mm, and the number of pores with the size 0.2-1.0 mm is 76.4%.

Structurae ne peut pas vous offrir cette publication en texte intégral pour l'instant. Le texte intégral est accessible chez l'éditeur. DOI: 10.35784/bud-arch.1887.
  • Informations
    sur cette fiche
  • Reference-ID
    10475989
  • Publié(e) le:
    25.11.2020
  • Modifié(e) le:
    25.11.2020
 
Structurae coopère avec
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine