Nanoindentation and nano-scratch testing on cement paste
Auteur(s): |
Salim Barbhuiya
(Senior Lecturer, Department of Engineering and Construction, University of East London, London, UK (corresponding author: ))
Bibhuti Bhusan Das (Associate Professor, Civil Engineering Department, National Institute of Technology Surathkal, Surathkal, India) |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Proceedings of the Institution of Civil Engineers - Construction Materials, mars 2024, n. 2, v. 177 |
Page(s): | 1-9 |