Multi-scale finite element analysis of the strengthening and damage behavior of carbides with different characteristics in nickel-based superalloys
Auteur(s): |
Qin Wang
Furong Liu Jinxia Song Yongwang Kang Yuhong Wu Dinggang Wang Chengbo Xiao |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Composite Structures, janvier 2025, v. 354 |
Page(s): | 118761 |
DOI: | 10.1016/j.compstruct.2024.118761 |
- Informations
sur cette fiche - Reference-ID
10811630 - Publié(e) le:
07.01.2025 - Modifié(e) le:
07.01.2025