Identification and mechanical properties of asphalt mastic-aggregate interface transition zone (ITZ) based on nanoindentation and AFM
Auteur(s): |
Zhaoyang Chu
Naisheng Guo Zhichen Wang Shuang Wang Zhanping You Xiangyuan Liu Enze Wu |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, janvier 2025, v. 461 |
Page(s): | 139898 |
DOI: | 10.1016/j.conbuildmat.2025.139898 |