Fracture toughness of fly ash-based geopolymer gels: Evaluations using nanoindentation experiment and molecular dynamics simulation
Auteur(s): |
Gideon A. Lyngdoh
Sumeru Nayak N. M. Anoop Krishnan Sumanta Das |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, novembre 2020, v. 262 |
Page(s): | 120797 |
DOI: | 10.1016/j.conbuildmat.2020.120797 |