Effect of sulfate attack on the composition and micro-mechanical properties of C-A-S-H gel in cement-slag paste: A combined study of nanoindentation and SEM-EDS
Auteur(s): |
Jun Yang
Qingjun Ding Gaozhan Zhang Dongshuai Hou Mingyu Zhao Jierong Cao |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, août 2022, v. 345 |
Page(s): | 128275 |
DOI: | 10.1016/j.conbuildmat.2022.128275 |