Comparison of Evolution of Pop-Out Damage by Mixed in Burnt Lime Nodules in Precast Concrete in Outside and Inside Exposure Conditions
Auteur(s): |
Dionys A. Van Gemert
Luc R. Taerwe Kristof P. Verreydt |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Restoration of Buildings and Monuments, avril 2018, n. 1, v. 23 |
Page(s): | 29-40 |
DOI: | 10.1515/rbm-2017-0002 |
Abstrait: |
In 2010 burnt lime blocks were accidentally mixed with limestone concrete aggregates at a Belgian limestone and lime production plant. The contaminated limestone aggregates were used in precast concrete factories. The concrete elements used in several constructions quickly showed pop-outs, caused by swelling of lime nodules. The appearance of pop-outs in suspected constructions was recorded. An extensive experimental program as well as on site observations have been made, to monitor the evolution of the pop-out phenomenon with time. The pop-out evolution in outside exposure conditions is compared to the evolution of pop-outs under inside climatic conditions. Outside, the phenomenon becomes marginal after about 2 years. In inside exposure conditions, the phenomenon still continues after 7 years, be it at a low rate. |
- Informations
sur cette fiche - Reference-ID
10531249 - Publié(e) le:
17.12.2020 - Modifié(e) le:
19.02.2021