Characterization of mechanical properties of shale constituent minerals using phase‐identified nanoindentation
Auteur(s): |
Jianting Du
(State Key Laboratory of Internet of Things for Smart City and Department of Civil and Environmental Engineering University of Macau Macau Macau SAR China)
Ka‐Veng Yuen (State Key Laboratory of Internet of Things for Smart City and Department of Civil and Environmental Engineering University of Macau Macau Macau SAR China) Andrew J. Whittle (Department of Civil and Environmental Engineering Massachusetts Institute of Technology Cambridge Massachusetts USA) Liming Hu (State Key Laboratory of Hydro‐Science and Engineering Tsinghua University Beijing China) Thibaut Divoux (MultiScale Material Science for Energy and Environment UMI 3466 CNRS‐MIT Cambridge Massachusetts USA) Jay N. Meegoda (State Key Laboratory of Hydro‐Science and Engineering Tsinghua University Beijing China) |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Computer-Aided Civil and Infrastructure Engineering, septembre 2024, n. 4, v. 40 |
Page(s): | 542-558 |
DOI: | 10.1111/mice.13346 |