12-years bending tensile stress corrosion of high-performance concrete under high salinity brine conditions
Auteur(s): |
Zhigang Ding
Hongfa Yu Haiyan Ma Haicheng Yang Xiaolun Hu Xiaoming Wang Zengzhuang Li Xianghui Han Meng Zhang |
---|---|
Médium: | article de revue |
Langue(s): | anglais |
Publié dans: | Construction and Building Materials, octobre 2024, v. 446 |
Page(s): | 137979 |
DOI: | 10.1016/j.conbuildmat.2024.137979 |