Galvanic Corrosion of ASTM A1010 Steel Connected to Common Bridge Steels
Author(s): |
Isaac G. Groshek
Matthew H. Hebdon |
---|---|
Medium: | journal article |
Language(s): | English |
Published in: | Journal of Materials in Civil Engineering (ASCE), August 2020, n. 8, v. 32 |
Page(s): | 04020193 |
DOI: | 10.1061/(asce)mt.1943-5533.0003131 |