Mechanical characterization of recycled tire rubber to be used as seismic isolation of the structure

 Mechanical characterization of recycled tire rubber to be used as seismic isolation of the structure
Autor(en): , ,
Beitrag für IABSE Symposium: Engineering for Progress, Nature and People, Madrid, Spain, 3-5 September 2014, veröffentlicht in , S. 1125-1131
DOI: 10.2749/222137814814067419
Preis: € 25,00 inkl. MwSt. als PDF-Dokument  
ZUM EINKAUFSWAGEN HINZUFÜGEN
Vorschau herunterladen (PDF-Datei) 0.12 MB

This paper discusses the results obtained by an experimental investigation aimed to the development of an innovative low-cost seismic base isolation pads using scrap car tires. The main idea consi...
Weiterlesen

Bibliografische Angaben

Autor(en):


Medium: Tagungsbeitrag
Sprache(n): Englisch
Tagung: IABSE Symposium: Engineering for Progress, Nature and People, Madrid, Spain, 3-5 September 2014
Veröffentlicht in:
Seite(n): 1125-1131 Anzahl der Seiten (im PDF): 7
Seite(n): 1125-1131
Anzahl der Seiten (im PDF): 7
Jahr: 2014
DOI: 10.2749/222137814814067419
Abstrakt:

This paper discusses the results obtained by an experimental investigation aimed to the development of an innovative low-cost seismic base isolation pads using scrap car tires. The main idea consists in realizing a new layer, by means of the recycled car tires, that replace large areas of the surrounding soil underneath the structure, or special elastomer based isolator between the soil and the basements. To this aim several tests have been conducted on specimens properly prepared from tires, in order to investigate the behavior of proposed system under compression and shear forces. The results reported here are related to the compression test and they were compared to the ones of common elastomer bearings (SREI). They show that at same strain levels, the instantaneous compression modulus values of RTP specimens are higher than that of the SREI values. The slope changes of RTP specimens start earlier and fail at much lower strains compared to SREI specimen. The high vertical stiffness of RTP layers combined with relatively low amount of steel content makes RTP layers stiffer and lower strength compared to SREI. Test results have shown that the friction between tire layers is sufficient to keep layers intact. RTP application so presents advantages such as low-technology no-cost pad, weight reduction, ease of handling, simple shear stiffness adjustment by changing the number of layers, and environmental benefits by recycling tires.