Evaluation of a Continuous Rigid Frame Bridge with Early Transverse Cracking

 Evaluation of a Continuous Rigid Frame Bridge with Early Transverse Cracking
Autor(en): ,
Beitrag für IABSE Symposium: Engineering for Progress, Nature and People, Madrid, Spain, 3-5 September 2014, veröffentlicht in , S. 550-557
DOI: 10.2749/222137814814028098
Preis: € 25,00 inkl. MwSt. als PDF-Dokument  
ZUM EINKAUFSWAGEN HINZUFÜGEN
Vorschau herunterladen (PDF-Datei) 0.18 MB

Early transverse cracking in the deck segment on interior pier of continuous rigid frame bridge constructed by balanced cantilever method is one of the dominant forms of bridge defects experience....
Weiterlesen

Bibliografische Angaben

Autor(en):

Medium: Tagungsbeitrag
Sprache(n): Englisch
Tagung: IABSE Symposium: Engineering for Progress, Nature and People, Madrid, Spain, 3-5 September 2014
Veröffentlicht in:
Seite(n): 550-557 Anzahl der Seiten (im PDF): 8
Seite(n): 550-557
Anzahl der Seiten (im PDF): 8
Jahr: 2014
DOI: 10.2749/222137814814028098
Abstrakt:

Early transverse cracking in the deck segment on interior pier of continuous rigid frame bridge constructed by balanced cantilever method is one of the dominant forms of bridge defects experience. These cracks often initiate soon after the deck segment on interior pier is constructed. Most of the past efforts addressing to transverse cracking have focused on causes and changes over the years in concrete material properties. However, bridge owners are more concerned with the impact of early transverse cracking on the performance and durability of the bridges. Thus bridge owners can make rational decisions vary from doing nothing to total rejection. This paper presents a comprehensive numerical study on a continuous rigid frame bridge with early transverse cracks in the China Western. The crack repair forms, crack numbers as well as crack spatial dimensions are considered as major causes in three 3D solid models with practical data. Analysis results showed that the existence of early transverse cracking in the deck segment on interior pier did not create much weakness in the structural static behavior.