Composite Stiffness of Asphalt and Deck and Its Influence on RD Joint

 Composite Stiffness of Asphalt and Deck and Its Influence on RD Joint
Autor(en): , , , ,
Beitrag für IABSE Conference: Elegance in structures, Nara, Japan, 13-15 May 2015, veröffentlicht in , S. 284-285
DOI: 10.2749/222137815815775060
Preis: € 25,00 inkl. MwSt. als PDF-Dokument  
ZUM EINKAUFSWAGEN HINZUFÜGEN
Vorschau herunterladen (PDF-Datei) 0.51 MB

Numerous fatigue cracks were observed recently in many long-time served orthotropic deck bridges. Especially the cracks initiating from rib-to-deck (RD) joint may produce asphalt surfacing damage a...
Weiterlesen

Bibliografische Angaben

Autor(en):





Medium: Tagungsbeitrag
Sprache(n): Englisch
Tagung: IABSE Conference: Elegance in structures, Nara, Japan, 13-15 May 2015
Veröffentlicht in:
Seite(n): 284-285 Anzahl der Seiten (im PDF): 8
Seite(n): 284-285
Anzahl der Seiten (im PDF): 8
Jahr: 2015
DOI: 10.2749/222137815815775060
Abstrakt:

Numerous fatigue cracks were observed recently in many long-time served orthotropic deck bridges. Especially the cracks initiating from rib-to-deck (RD) joint may produce asphalt surfacing damage and hence cause impact on traffic safety. For fatigue evaluation of RD joints, in most current design specifications, the asphalt surfacing is just treated as a layer dispersing wheel loads and the effect of composite stiffness of asphalt surfacing and deck plate is neglected. In this study, Full size experiment for 2 spans orthotropic bridge deck with asphalt surfacing were carried out to investigate the stress distribution around RD joints and a special indoor asphalt heating and cooling system was employed to study the real stress distribution around RD joint with considering asphalt temperature variation. The experiment results show that the most critical transversal load cases for fatigue damage of RD joint are wheel load ride on the RD joint and located around the adjacent RD joint. Moreover the transversal stresses around RD joint are significantly sensitive to the asphalt temperature and the most sensitive temperature range is 5 degree Celsius to 35 degree Celsius.

Stichwörter:
Temperatur Ermüdungsriß