0
  • DE
  • EN
  • FR
  • Internationale Datenbank und Galerie für Ingenieurbauwerke

Anzeige

Assessment of the shear strength of existing post-tensioned bridges

 Assessment of the shear strength of existing post-tensioned bridges
Autor(en): , ,
Beitrag für IABSE Symposium: Engineering the Future, Vancouver, Canada, 21-23 September 2017, veröffentlicht in , S. 2120-2125
DOI: 10.2749/vancouver.2017.2120
Preis: € 25,00 inkl. MwSt. als PDF-Dokument  
ZUM EINKAUFSWAGEN HINZUFÜGEN
Vorschau herunterladen (PDF-Datei) 0.19 MB

The assessment of existing structures is becoming more and more important in the field of activity of a structural engineer. To get more information about the load-carrying behaviour of shear criti...
Weiterlesen

Bibliografische Angaben

Autor(en): (TU Wien, Vienna, Austria)
(TU Wien, Vienna, Austria)
(TU Wien, Vienna, Austria)
Medium: Tagungsbeitrag
Sprache(n): Englisch
Tagung: IABSE Symposium: Engineering the Future, Vancouver, Canada, 21-23 September 2017
Veröffentlicht in:
Seite(n): 2120-2125 Anzahl der Seiten (im PDF): 6
Seite(n): 2120-2125
Anzahl der Seiten (im PDF): 6
Jahr: 2017
DOI: 10.2749/vancouver.2017.2120
Abstrakt:

The assessment of existing structures is becoming more and more important in the field of activity of a structural engineer. To get more information about the load-carrying behaviour of shear critical bridge structures an experimental campaign on large-scale post-tensioned specimen was carried out. With the aid of DIC it was possible to measure the crack kinematics of the critical shear crack during the whole test. Thus, an evaluation of different shear-transfer actions were performed. Based on these results a shear design concept – including different shear models – for post-tensioned bridge girders with a very low amount of transverse reinforcement was proposed. The approach was used to evaluate the shear strength of a real existing post-tensioned bridge. Based on the suggested concept a cost-extensive strengthening of the webs were prevented.

Stichwörter:
Brücken Scherfestigkeit Bewertung