Water Resistance of Acrylic Adhesive Tapes for Rooftop Fastening
Autor(en): |
Klára V. Machalická
Petr Sejkot Miroslav Vokáč Petr Pokorný Vera Obradović |
---|---|
Medium: | Fachartikel |
Sprache(n): | Englisch |
Veröffentlicht in: | Buildings, 19 Juni 2024, n. 6, v. 14 |
Seite(n): | 1636 |
DOI: | 10.3390/buildings14061636 |
Abstrakt: |
Rooftop solar modules are usually held in place by racks or frames that are mechanically attached to a roof structure and/or by heavyweight, ballasted footing mounts. These mounts ensure that the panel system remains in position against wind load. However, mechanical connectors create penetrations into the water-resistant layer of the roof, whereas ballasted footing mounts cause a significant additional load on the load-bearing structure of roof. For these reasons, adhesive connection seems to be a beneficial solution. Acrylic adhesive tapes, marked as VHBTM, may provide sufficient strength, and they have no need for mechanical fasteners or ballast. Acrylic adhesive tapes also provide a comfortable, fast, and efficient bonding process with no curing compared to liquid adhesives. On the other hand, resistance to water at load-bearing joints has not been sufficiently studied yet and could be critical for connections exposed to the outdoor environment. The present study aims at the determination of water resistance and durability of the VHBTM tapes from the GPH series, which are typically used to bond a variety of substrates including many metals. The mechanical properties and failure modes are compared for the specimens before and after a 21-day immersion in water. A significant reduction in strength was observed, depending on the substrate material. The study of chemical changes in the acrylic tape and in its leachate through infrared spectroscopy (FT-IR), X-ray fluorescence, and X-ray diffraction analyses clarified the reduction in mechanical properties. The selected VHBTM tape demonstrated strong resistance to the effects of water. However, the overall strength of the joint after immersion was significantly impacted by the decrease in adhesion to a specific substrate. |
Copyright: | © 2024 by the authors; licensee MDPI, Basel, Switzerland. |
Lizenz: | Dieses Werk wurde unter der Creative-Commons-Lizenz Namensnennung 4.0 International (CC-BY 4.0) veröffentlicht und darf unter den Lizenzbedinungen vervielfältigt, verbreitet, öffentlich zugänglich gemacht, sowie abgewandelt und bearbeitet werden. Dabei muss der Urheber bzw. Rechteinhaber genannt und die Lizenzbedingungen eingehalten werden. |