Research on Hybrid FRP–Steel-Reinforced Concrete Slabs under Blast Load

Autor(en):

ORCID
Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: Buildings, , n. 4, v. 13
Seite(n): 1058
DOI: 10.3390/buildings13041058
Abstrakt:

The service environment of civil air defense engineering structures is relatively harsh, and the corrosion of steel bars is the main reason for reducing the durability of concrete structures in civil air defense engineering. A hybrid FRP–steel-reinforced concrete (hybrid-RC) structure has excellent durability. Therefore, it is a good choice to apply hybrid-RC to civil air defense engineering structures. In order to study the blast resistance of hybrid-RC structures, close blast and contact blast experiments were carried out on hybrid-RC slabs, steel-reinforced concrete (SRC) slabs and GFRP-reinforced concrete (GRC) slabs. For the close blast experiment, the steel reinforcement in the SRC slab first entered the plasticity stage, whereas the GFRP reinforcement in the hybrid-RC slab was in the elastic stage under the close blast. Therefore, the capacity to dissipate energy through the vibration in the hybrid-RC slab was better than that of the SRC slab. The residual deformation in the hybrid-RC slab after the close blast experiment was smaller than that of the SRC slab. The Blast Recovery Index (BRI) was introduced to evaluate the recovery capacity of the concrete slab after the close blast, and damage assessment criteria for the hybrid-RC slabs were proposed according to the maximum support rotation θm and BRI. There was little difference in the size of the local damage in the hybrid-RC slab and the SRC slab under the contact blast. However, since the GFRP reinforcement was still in the elastic stage and the steel reinforcement was plastic after the contact blast, the ratio of the residual bearing capacity to the original bearing capacity in the hybrid-RC concrete slab would be larger than that of the SRC slab. The prediction formula for the top face diameter D and blasting depth L of the hybrid-RC slab was obtained through dimensionless analysis. This research can provide a reference for the anti-blast design of hybrid-RC slabs.

Copyright: © 2023 by the authors; licensee MDPI, Basel, Switzerland.
Lizenz:

Dieses Werk wurde unter der Creative-Commons-Lizenz Namensnennung 4.0 International (CC-BY 4.0) veröffentlicht und darf unter den Lizenzbedinungen vervielfältigt, verbreitet, öffentlich zugänglich gemacht, sowie abgewandelt und bearbeitet werden. Dabei muss der Urheber bzw. Rechteinhaber genannt und die Lizenzbedingungen eingehalten werden.

  • Über diese
    Datenseite
  • Reference-ID
    10728506
  • Veröffentlicht am:
    30.05.2023
  • Geändert am:
    01.06.2023
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine