Numerical simulation of mechanical properties and damage process of carbon nanotube concrete under triaxial compression and splitting conditions

Autor(en):
ORCID



Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: Electronic Journal of Structural Engineering, , n. 3, v. 24
Seite(n): 39-45
DOI: 10.56748/ejse.24617
Abstrakt:

To investigate the mechanical properties and failure processes of carbon nanotube concrete, a three-dimensional meso-scale finite element model of concrete was constructed. Using ABAQUS software, numerical simulations were conducted on concrete samples with different carbon nanotube concentrations under triaxial compression and splitting conditions. The results indicate that under splitting conditions, the failure of the specimens initially occurs along the loading direction from both ends, with few cracks and slow propagation. Subsequently, the cracks rapidly expand, penetrating the entire specimen, leading to the formation of a macro-fracture surface with a crack aligned with the loading direction. This failure mode manifests as a straight crack. At the same loading rate, the tensile strength of the specimens with different carbon nanotube concentrations increases to varying degrees during splitting failure, with a maximum increase of 45.10% to 4.15 MPa. nder triaxial compression conditions, the main failure mode of the specimens exhibits shear failure characteristics. As the confining pressure gradually increases, the failure angle of the specimens enlarges. Under low confining pressure, there are fewer wing-shaped tensile cracks at the shear failure surface of the specimens. As the confining pressure increases, irregular shear failures and multiple shear planes appear in the specimens, resulting in more complex failure modes. For specimens with the same carbon nanotube concentration, the triaxial compressive strength of carbon nanotube concrete specimens increases with increasing confining pressure. The triaxial compressive strengths of the specimens under confining pressures of 5 MPa, 10 MPa, 15 MPa, and 20 MPa are 90.48 MPa, 122.72 MPa, 137.22 MPa, and 172.65 MPa, with strength increases of 35.63%, 51.66%, and 90.81%, respectively.

Structurae kann Ihnen derzeit diese Veröffentlichung nicht im Volltext zur Verfügung stellen. Der Volltext ist beim Verlag erhältlich über die DOI: 10.56748/ejse.24617.
  • Über diese
    Datenseite
  • Reference-ID
    10805064
  • Veröffentlicht am:
    10.11.2024
  • Geändert am:
    10.11.2024
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine