Nanotechnology and construction: use of nanoindentation measurements to predict macroscale elastic properties of high strength cementitious composites

Autor(en):


Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: Revista IBRACON de Estruturas e Materiais, , n. 3, v. 5
Seite(n): 284-295
DOI: 10.1590/s1983-41952012000300002
Abstrakt:

This paper aims to present the experimental results involving the use of nanoindentation measurements and prediction of macroscale elastic properties of high performance cementitious composites (HPCC). The elastic properties of HPCC mixture were evaluated at different length scales by nanoindentation (microscale), and elastic moduli and compressive strength tests (macroscale). The nanoindentation results, obtained by grid indentation with subsequent phase deconvolution, were complemented by an independent porosimetry test and inserted into a two-step analytical homogenization scheme to predict the overall macroscale properties. The final results show that the presented method allows a reliable advanced prediction of HPCC elastic properties indicating, thus, that inserting nanotechnology in the concrete industry can be promising, since it would allow the production of a more predictable composite in an easier and less expensive way.

Structurae kann Ihnen derzeit diese Veröffentlichung nicht im Volltext zur Verfügung stellen. Der Volltext ist beim Verlag erhältlich über die DOI: 10.1590/s1983-41952012000300002.
  • Über diese
    Datenseite
  • Reference-ID
    10413593
  • Veröffentlicht am:
    12.02.2020
  • Geändert am:
    12.02.2020
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine