Glass Fiber for Improved Behavior of Light Expanded Clay Aggregate Concrete Beams: An Experimental Study

Autor(en):

ORCID
Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: Frattura ed Integrità Strutturale, , n. 65, v. 17
Seite(n): 1-16
DOI: 10.3221/igf-esis.65.01
Abstrakt:

Concrete developed from light expanded clay aggregate (LECA) and glass fiber has good performance, durability, and sustainability. Towards this, the experimental investigation was designed to study cubes, cylinders, and simply supported beams. Four mixtures had LECA volume of 0%, 75%, 85%, and 95% as coarse aggregate replacement and glass fiber content volume of 2% (N, L75, L85, and L95), and the other two mixtures had 75% LECA and glass fiber content of 1% and 1.5% (L75-F1 and L75-F1.5). Results compared to normal concrete showed the weight reduction of samples while adding more glass fiber caused slump reduction in contrast to LECA. Increasing glass fiber volume in the mixture had a negative influence on tensile strength while causing compressive strength enhancement. Moment resistance and energy absorption capacity of L85 were enhanced by 7.5% and 10.3%, respectively. For L75-F1 specimens, the beam stiffness and ductility were enhanced by 14.8% and 14.3%, respectively.  

Structurae kann Ihnen derzeit diese Veröffentlichung nicht im Volltext zur Verfügung stellen. Der Volltext ist beim Verlag erhältlich über die DOI: 10.3221/igf-esis.65.01.
  • Über diese
    Datenseite
  • Reference-ID
    10739838
  • Veröffentlicht am:
    01.09.2023
  • Geändert am:
    01.09.2023
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine