Effect of salt water ageing on the degradation of steel‐composite bonded interfaces

Autor(en): (TU Delft Delft Netherlands)
(TU Delft Delft Netherlands)
(Tree Composites Delft Netherlands)
(Tree Composites Delft Netherlands)
(TU Delft Delft Netherlands)
Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: ce/papers, , n. 3-4, v. 6
Seite(n): 293-296
DOI: 10.1002/cepa.2646
Abstrakt:

This work aims to investigate the long‐term effect of sea water conditions on the steel‐composite interface. The degradation of the steel‐composite bonded interface was investigated using fracture tests in coupon specimens. Specimens were manufactured and placed for ageing in a salt water solution to simulate the degradation of the bi‐material interface in offshore environment. Four‐point end notched flexure (4ENF) tests were performed to access the interface fracture behavior under quasi‐static loadings. Results of non‐aged and aged specimens show negligible degradation of the interface fracture properties after 69 days of immersion. In addition, steel plates were coated with resin and placed for ageing. The corrosion of uncoated and coated steel surfaces was inspected using optical microscopy. Results showed that the coated steel surface is susceptible to the environmental degradation. This indicates that the steel‐composite interface bonding will degrade after moisture reaches the steel surface.

Structurae kann Ihnen derzeit diese Veröffentlichung nicht im Volltext zur Verfügung stellen. Der Volltext ist beim Verlag erhältlich über die DOI: 10.1002/cepa.2646.
  • Über diese
    Datenseite
  • Reference-ID
    10767230
  • Veröffentlicht am:
    17.04.2024
  • Geändert am:
    17.04.2024
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine