0
  • DE
  • EN
  • FR
  • Internationale Datenbank und Galerie für Ingenieurbauwerke

Anzeige

Durability, Capillary Rise and Water Absorption Properties of a Fiber-Reinforced Cement-Stabilized Fly Ash–Stone Dust Mixture

Autor(en):




ORCID

ORCID


Medium: Fachartikel
Sprache(n): Englisch
Veröffentlicht in: Infrastructures, , n. 2, v. 9
Seite(n): 17
DOI: 10.3390/infrastructures9020017
Abstrakt:

The management of unutilized fly ash poses challenges due to concerns about storage and its potential groundwater contamination. Within the road industry, where the bulk utilization of fly ash is feasible, its unsuitability for use in the base and sub-base layers of pavements due to its low strength and a high proportion of fine particles has been a limitation. The incorporation of stone dust alongside fly ash, treated with lime or cement, yields superior strength and stiffness. Apart from strength, the stabilized mix’s durability, capillary rise, and water absorption properties are crucial for determining its suitability for pavement applications. Observations from this study reveal that fiber-reinforced cement-stabilized fly ash–stone aggregate specimens treated with 4% and 6% cement, with and without fibers, met the limiting mass loss of 20%, as specified in IRC SP: 89. The mass loss decreases with an increase in cement and fiber content. However, the capillary rise in the mixes increases with a higher percentage of fly ash and fiber content but decreases with increased cement content. Cement addition results in a reduction in water absorption; however, the addition of fibers results in an increase in water absorption. A linear correlation has been established between mass loss and UCS and IDT, which can be used to evaluate the suitability of materials for the structural layer without conducting a wet–dry durability test, which typically takes one month. This study proposes that cement-stabilized fly ash and stone aggregate mixtures with 4% and 6% cement can be used as the subbase and base of pavement based on wet–dry mass loss criteria and water absorption criteria. Observations from this study reveal that fiber-reinforced cement-stabilized fly ash–stone aggregate specimens treated with 4% and 6% cement, with and without fibers, met the limiting mass loss of 20%, as specified in IRC SP: 89. The mass loss decreases with an increase in cement and fiber content. However, the capillary rise in the mixes increases with a higher percentage of fly ash and fiber content but decreases with increased cement content. Cement addition results in reduction in water absorption. However, the addition of fibers results in increase in water absorption. A linear correlation is established between mass loss and UCS and IDT, which can be used to evaluate the suitability of materials for the structural layer without conducting wet–dry durability tests, which take one month. This study proposes that cement-stabilized fly ash and stone aggregate mixtures with 4% and 6% cement can be used as the subbase and base of pavement based on wet–dry mass loss criteria and water absorption criteria.

Copyright: © 2024 the Authors. Licensee MDPI, Basel, Switzerland.
Lizenz:

Dieses Werk wurde unter der Creative-Commons-Lizenz Namensnennung 4.0 International (CC-BY 4.0) veröffentlicht und darf unter den Lizenzbedinungen vervielfältigt, verbreitet, öffentlich zugänglich gemacht, sowie abgewandelt und bearbeitet werden. Dabei muss der Urheber bzw. Rechteinhaber genannt und die Lizenzbedingungen eingehalten werden.

  • Über diese
    Datenseite
  • Reference-ID
    10761379
  • Veröffentlicht am:
    15.03.2024
  • Geändert am:
    25.04.2024
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine