Determining Hardness and Elastic Modulus of Asphalt by Nanoindentation
Autor(en): |
Rafiqul A. Tarefder
(Assistant Professor, Dept. of Civil Engineering, Univ. of New Mexico, MSC01 1070, Albuquerque, NM 87131 (corresponding author).)
Arif M. Zaman (Assistant Professor, Dept. of Civil Engineering, Univ. of New Mexico, MSC01 1070, Albuquerque, NM 87131 (corresponding author).) Waheed Uddin (Assistant Professor, Dept. of Civil Engineering, Univ. of New Mexico, MSC01 1070, Albuquerque, NM 87131 (corresponding author).) |
---|---|
Medium: | Fachartikel |
Sprache(n): | Englisch |
Veröffentlicht in: | International Journal of Geomechanics, Juni 2010, n. 3, v. 10 |
Seite(n): | 106-116 |
DOI: | 10.1061/(asce)gm.1943-5622.0000048 |