Abstrakt:

Granulated blast‐furnace slag sand (BFS) has the potential to be used as an alternative to fine aggregates in concrete production. The interface between the cement paste and the aggregate in concrete is densified when BFS is used, due to the hydrates that are generated by its latent hydraulicity. This fact suggests that the crack resistance of concrete, which is closely related to the conditions at the aggregate interface, would be enhanced by the use of BFS. The fracture energy (GF) of concrete under flexural stress is here measured to evaluate the crack resistance of concrete made using BFS. BFS samples from three different steel mills in Japan are used as the fine aggregates for concrete production, and mountain sand is used as a natural sand for comparison. Compressive strength, static modulus of elasticity, and fracture energy tests are conducted at the material ages of 28 and 91 days. The GF of the BFS concretes increase with increasing compressive strength; on the other hand, the GF of the concrete made using mountain sand decrease. Thus, it is concluded that BFS concrete has superior properties to concrete made using natural sand in terms of the crack resistance under flexural stress, especially in high‐strength regions for large material ages.

Structurae kann Ihnen derzeit diese Veröffentlichung nicht im Volltext zur Verfügung stellen. Der Volltext ist beim Verlag erhältlich über die DOI: 10.1002/cepa.2832.
  • Über diese
    Datenseite
  • Reference-ID
    10750370
  • Veröffentlicht am:
    14.01.2024
  • Geändert am:
    14.01.2024
 
Structurae kooperiert mit
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine