A review of key developments and pertinent issues in nanoindentation testing of fibre reinforced plastic microstructures

Author(s):


Medium: journal article
Language(s): English
Published in: Composite Structures, , v. 180
Page(s): 782-798
DOI: 10.1016/j.compstruct.2017.08.004
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.compstruct.2017.08.004.