Energy absorption and damage mechanisms in progressive crushing of corrugated NCF laminates: Fractographic analysis

Author(s):


Medium: journal article
Language(s): English
Published in: Composite Structures, , v. 110
Page(s): 110-117
DOI: 10.1016/j.compstruct.2013.11.001
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.compstruct.2013.11.001.