Effect of glass fiber sheet in adhesive on the bond and galvanic corrosion behaviours of CFRP-Steel bonded system

Author(s):




Medium: journal article
Language(s): English
Published in: Composite Structures, , v. 259
Page(s): 113218
DOI: 10.1016/j.compstruct.2020.113218
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.compstruct.2020.113218.