Cyclic testing of beam-to-column connections with weld defects and assessment of safety of numerically modeled connections from brittle fracture

Author(s):


Medium: journal article
Language(s): English
Published in: Engineering Structures, , n. 12, v. 22
Page(s): 1596-1608
DOI: 10.1016/s0141-0296(99)00115-7
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/s0141-0296(99)00115-7.